this post was submitted on 15 Sep 2024
34 points (97.2% liked)

3DPrinting

15548 readers
182 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I have been trying for many hours now to print this circular model, but have been running into inconsistent extrusion and stringing. just before printing this, I successfully printed a set of Hextraction tiles, so I'm not really sure what the issue is. I also printed this model successfully in the past with the same settings.

I am using a Sovol SV06 with stock firmware, and PLA with the hotend at 195° C.

I also did a full calibration to see if that would fix the issue, and it did not.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 2 points 1 month ago (1 children)

That was a typo, sorry, it was set at 195 C

[–] [email protected] 2 points 1 month ago* (last edited 1 month ago)

All good! It's the same situation as I described and I see that increasing temps did help. It's good to do a temperature tower test for quality and also a full speed test after that. After temperature calibration, print a square that is only 2 or 3 bottom layers that covers the entire bed at full speed or faster. (It's essentially a combined adhesion/leveling/extrusion volume/z offset test, but you need to understand what you are looking at to see the issues separately.)

If you have extrusion problems, the layer line will start strong from the corners, get thin during the acceleration and may thicken up again at the bottom of the deceleration curve. A tiny bit of line width variation is normal, but full line separation needs attention.