this post was submitted on 21 Apr 2024
45 points (97.9% liked)

3DPrinting

15577 readers
73 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Anyone have any idea what might cause this sort of issue on PLA? I run into it frequently, but pretty much only when all of the following points are true:

  • the print has multiple parts, so the extruder spends a decent amount of time off of any given part (only one part from this print is pictured)
  • the affected part(s), like the picture above, have a relatively steep outward overhang, extending over the build plate
  • the outward overhang part is relatively narrow, as seen from a top view

This is from a printer with a 4028 fan (i.e. pretty massive airflow, server type fan) so even the 35-45% (based on layer time) I have it currently set at is more than 100% with single/dual 5015's or etc.

I guess my other option is to try supports, but this doesn't really seem like a situation where supports should be needed. Anyone ever had a similar problem and solved it without just turning the speed waaaayyyyyy down?

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 3 points 6 months ago

How fast are you trying to print? Does it behave differently if you slow down?

One of the reasons prints can shrink like this is that the speed is essentially stretching the plastic as it comes out the nozzle, like a rubber band. As the plastic settles that tension pulls it together.

I doubt moisture is the issue, PLA doesn't actually absorb water very quickly.

Also, have you done a temperature tower and flow calibrarion for this filament?