mellitiger

joined 1 year ago
[โ€“] [email protected] 2 points 9 months ago* (last edited 9 months ago)

You are absolutely right, just for clarity:

Chromium needs to be > 12 weight-%. If you take 18 w-% Cr and 8 w-% Ni you get an austenitic steel which is (normally) neither magnetic nor able to be hardened.

And if you add 12 w-% Cr, you remove 12 w-% Fe. So formally this is right-ish too...

[โ€“] [email protected] 0 points 1 year ago

Thanks for sharing - and there are some parts that seem to be missing. Starting with Part 4 ;)