this post was submitted on 23 Nov 2024
1 points (100.0% liked)

Electronics

2080 readers
2 users here now

Projects, pictures, industry discussions and news about electronic engineering & component-level electronic circuits.

Rules

1: Be nice.

2: Be on-topic (eg: Electronic, not electrical).

3: No commercial stuff, buying, selling or valuations.

4: No circuit design or repair, tools or component questions.

5: No excessively promoting your own sites, social media, videos etc.


Ask questions in https://discuss.tchncs.de/c/askelectronics


founded 2 years ago
MODERATORS
 

Me a few days ago, shopping on Amazon: "All the component and jumper wire leads are going to be on the bottom anyway; why shouldn't I get a pack of single-sided breadboards for $6.25 instead of double-sided ones for $10?"

Me today, after having lifted three pads off the damn board in 10 minutes: "Oh, that's why."

Get the double-sided breadboards; they're worth it.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 0 points 1 month ago

Double sided perfboards way more often than not don't have plated vias. The vast majority are just etched from a 2 layer blank without any post processing.

You would have to solder specifically on both sides in order to increase the strength.

But yes pads lifting is almost exclusively from dumping way too much heat in it. Because there is no plated through hole, it also has ~1/4 of the thermal mass so it is easier to overheat and damage the adhesive.