ErgoMechKeyboards
Ergonomic, split and other weird keyboards
Rules
Keep it ergo
Posts must be of/about keyboards that have a clear delineation between the left and right halves of the keyboard, column stagger, or both. This includes one-handed (one half doesn't exist, what clearer delineation is that!?)
i.e. no regular non-split¹ row-stagger and no non-split¹ ortholinear²
¹ split meaning a separation of the halves, whether fixed in place or entirely separate, both are fine.
² ortholinear meaning keys layed out in a grid
No Spam
No excessive posting/"shilling" for commercial purposes. Vendors are permitted to promote their products/services but keep it to a minimum and use the [vendor] flair. Posts that appear to be marketing without being transparent about it will be removed.
No Buy/Sell/Trade
This subreddit is not a marketplace, please post on r/mechmarket or other relevant marketplace.
Some useful links
- EMK wiki
- Split keyboard compare tool
- Compare keycap profiles Looking for another set of keycaps - check this site to compare the different keycap profiles https://www.keycaps.info/
- Keymap database A database with all kinds of keymap layouts - some of them fits ergo keyboards - get inspired https://keymapdb.com/
view the rest of the comments
Thank you very much for answering.
I believe the pcb is lead free as I got it from jlcpcb and they have it written in the package of each side that they’re lead free. The solder itself is also lead free from a reputable electronic store near where I live so I think it should be safe. I live in an apartment so it will be tricky to do it outside, I may try to solder it where my cooktop is as I can turn on the range hood to suck the bad air up.
Do I need to clean the flux that comes with the solder or it’s not that big of a deal? I’d expect that touching it when dry would be safe as well right?
Look at your solder spool, and see if it says multi-core? If you're not sure go ahead and show us a photo or write out the type of solder you're using.
You need flux and solder together, flux prevents the board from oxidizing especially when you heat it up, it makes it easier for the metal to flow. A lot of solder has the flux built into the solder itself. When you put a hot soldering iron up to the solder and you see the smoke, the smoke is the flux, the antioxidation element not the metal. The metal does not smoke
If you're using flux in addition to your solder, like a flux paste or a flux gel or a flux liquid you brush on, that's fine too. Just don't breathe the fumes.
If you have a real n95 or n100 mask kicking around, wear that, do your soldering next to an open window or under your vent hood, let it keep venting after you're done for a couple minutes. And wash your hands and you'll be fine
The solder I’m using is this one: https://www.jaycar.com.au/lead-free-solder-1mm-15g-hobby-tube/p/NS3092?pos=1&queryId=f28fc8a65a86eab148b5f9ae9b304dcc
This is the description:
1mm lead free resin core solder. Contains tin and copper 99.3/0.07
Thanks again for the advice. I’ll wear a mask when soldering.
Lot of good points here. I work in electronics manufacturing so I'll add on a bit. Yes, much of what has been explained about solder and flux is correct. I will caution about trying something like conformal coating a board in this setting. It is hard to work through and can beat up your iron. Lead free is great but sucks for working it into the joints. It just doesn't heatt the same. Even IPC build standards have explicit instructions about visual inspections of non leaded joints looking like shit.
If you are planning to coat the board, I would do outdoors as well. Extraction fans are great for general soldering but we use fume hoods for conformal coat. Just something to keep in mind.